DMLS Materials & Specifications
|
Material |
Characteristics |
Applications |
|
Stainless Steel 17-4 (GP1) |
20 or 40 Micron Layers 20-25 HRC As Built 45 HRC Post Hardened Max Temp - 550°C, 1022°F |
|
|
Stainless Steel 15-5 (PH1) |
20 or 40 Micron Layers 30-35 HRC As Built 40 HRC Post Hardened Max Temp - 460°C, 860°F |
|
|
Cobalt Chrome (MP1) |
20 or 40 Micron Layers 40-45 HRC As Built Max Temp - 1150°C, 2100°F |
e.g. Turbines and other parts for engines, cutting parts
|
|
Maraging Steel (MS1) (Tooling Steel) |
40 Micron Layers 33-37 HRC As Built 50-54 HRC Post Hardened Max Temp - 400°C, 750°F |
|
|
Bronze (DM20) |
20 or 40 Micron Layers 115 HV As Built Max Temp - 400°C, 750°F |
|
|
Titanium Alloy (Ti64) |
20-60 Micron Layers 41-44 HRC As Built Max Temp - 350°C, 660°F |
e.g. Structural and engine components for aerospace and motorsport applications
|
|
Aluminum (AlSi10mg) |
30 Micron Layers 120 ± 5 HBW As Built 112 ± 5 HBW Post Hardened |
e.g. Motorsport applications |
|
Nickel Alloy (IN718) (Inconel) |
20 or 40 Micron Layers 30 HRC As Built 47 HRC Post Hardened Max Temp - 650°C, 1200°F |
|